Rene 41 - Precipitation hardened nickel alloy with excellent strength through 1600°F. Used for gas turbine and missile hot components, including bolting and springs.
|
|
Cr |
Ni |
Mo |
Co |
Al |
Ti |
B |
C |
Fe |
Mn |
Si |
S |
Cu |
|
MIN |
18 |
-- |
9 |
10 |
1.4 |
3 |
0.003 |
-- |
-- |
-- |
-- |
-- |
-- |
|
MAX |
20 |
Balance |
10.5 |
12 |
1.8 |
3.3 |
0.01 |
0.12 |
5 |
0.1 |
0.5 |
0.015 |
0.5 |
Rene 41 is an age hardening nickel base superalloy with exceptional strength from room temperature through about 1600°F. The alloy is sensitive to strain age cracking during welding. Sound welds can be made by the resistance and electron beam methods. GTAW using DC straight polarity requires good joint fit-up and cooling by means of copper backup bars or water-cooled fixtures. René 41 should be in the fully solution treated condition prior to welding. After welding the assembly should be solution treated using rapid heating and cooling rates through the 1200-1600°F range, followed by aging.
Mechanical properties vary with the solution and aging treatments. Higher solution temperatures result in better room temperature ductility and elevated temperature creep-rupture strength. Lower solution temperatures give higher tensile strengths. Two commonly used heat treatments are:
1. Solution treat: 2150°F 4 hours, air cool. Age: Reheat 1650 °F 4 hours, air cool.
2. Solution treat: 1975 °F 4 hours, air cool. Age: Reheat 1400°F 16 hours, air cool.
Common Trade Names :Rene 41 Alloy
AMS 5545, AMS 5712, AMS 5713, AMS 5800, EN 2.4973, GE B50T59, GE B50TF109, GE B50TF76, UNS N07041, Werkstoff 2.4973
·Exceptionally high strength
·Oxidation resistant through 1800°F
·Jet engine hot components
·Missile components
·Bolting
·Springs